Read Sharp MX-4140N / MX-4141N / MX-5140N / MX-5141N (serv.man117) Technical Bulletin online
Pg. 2 of 3
On the other hand, however, the warp of the paper, caused when using Plain
Paper, tends to be slightly bigger due to the influence of the Delivery Sponge.
For this reason, when the MX‐FNX9 is installed to the Virgo2, in some cases, the
warped paper cannot enter the paper entrance of the Punch Unit* or the Dummy
Punch Unit*, resulting in a Paper Jam (POD1_S) depending on the paper type.
*Due to the narrow paper entrance section (height) of the Punch Unit or the
dummy punch unit paper guide. (see below)
[Countermeasure]
For the Permanent countermeasure, the plan about changing the shape of the
Paper Unit from September 2012 production is now ongoing.
As soon as the detail is decided, a Technical Report will be issued.